Product Code: NACLP23-41-5
- Price:
- £99.80
50 In Stock
There is not enough stock to fulfil your order, either reduce the amount to the number available, or if you do require more, proceed and you will be contacted by a member of the sales team.
Product Code NACLP23-41-5
IR Polished Sodium Chloride (NaCl) optical window
23mm x 41mm x 5mm
Rectangular - A popular size for FTIR spectroscopy
Undrilled for use alone or as a pair with NACLP23-41-5-D