Silicon FZ - Circular Windows

Silicon FZ - Circular Windows

Circular Silicon Float Zone Windows from Stock.

Optical grade Silicon is normally specified with a resistivity of 5 to 40 ohm-cm which is higher than most semiconductor applications. The windows listed here are made from FZ, Float Zone material which does not have this Si-O absorption at arount 9 microns wavelength.

Very high resistivity material can be supplied on special order, particularly for TeraHertz applications.

Click for Technical Data on Silicon

  •  10.0mm x 2.0mm

    10.0mm x 2.0mm

    Product Code SIFZP10-2 IR Polished Silicon (Si) optical window 10mm Ø x 2mm FZ, Float-Zone Grade (no absorption band at 9μm) ...

    73 In Stock. £16.00 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details
  •  12.0mm x 1.0mm

    12.0mm x 1.0mm

    Product Code SIFZP12-1 IR Polished Silicon (Si) optical window 12mm Ø x 1mm FZ, Float-Zone Grade (no absorption band at 9μm) ...

    87 In Stock. £15.75 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details
  •  13.0mm x 1.0mm

    13.0mm x 1.0mm

    Product Code SIFZP13-1 IR Polished Silicon (Si) optical window 13mm Ø x 1mm FZ, Float-Zone Grade (no absorption band at 9μm) ...

    156 In Stock. £15.75 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details
  •  15.0mm x 1.0mm

    15.0mm x 1.0mm

    Product Code SIFZP15-1 IR Polished Silicon (Si) optical window 15mm Ø x 1mm FZ, Float-Zone Grade (no absorption band at 9μm)   ...

    130 In Stock. £21.00 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details
  •  25.4mm x 0.5mm

    25.4mm x 0.5mm

    Product Code SIFZP25.4-0.5 IR Polished Silicon (Si) optical window 25.4mm Ø x 0.5mm (1 inch Ø x 0.5mm) FZ, Float-Zone Grade (no...

    59 In Stock. £31.50 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details
  •  25.4mm x 1.0mm

    25.4mm x 1.0mm

    Product Code SIFZP25.4-1 IR Polished Silicon (Si) optical window 25.4mm Ø x 1mm (1 inch Ø x 1mm) FZ, Float-Zone Grade (no...

    302 In Stock. £31.50 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details
  •  30.0mm x 2.0mm

    30.0mm x 2.0mm

    Product Code SIFZP30-2 IR Polished Silicon (Si) optical window 30mm Ø x 2mm FZ, Float-Zone Grade (no absorption band at 9μm)   ...

    23 In Stock. £47.25 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details
  •  30.0mm x 3.0mm

    30.0mm x 3.0mm

    Product Code SIFZP30-3 IR Polished Silicon (Si) optical window 30mm Ø x 3mm FZ, Float-Zone Grade (no absorption band at 9μm)   ...

    36 In Stock. £50.40 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details