Silica Glass UV - Rectangular Windows

UV Grade Fused Silica - Rectangular Windows.

Fused Silica normally contains OH which causes a strong absorption centred on 2.7μm limiting transmission to 2.2μm and restricting usefulness for IR applications. Grades with low OH (typically less than 10ppm) are available and they can be used effectively to 3.0μm.

These windows are made from UV grade material which contains OH and are useful from 0.18μmto 2.2μm.

Click for Technical Data on Silica Glass

  • 26.0 x 24.0 x 1.0mm

    26.0 x 24.0 x 1.0mm

    Product Code:  FSUVP26-24-1 UV Grade polished Fused Silica (SiO2) rectangular optical window 26mm x 24mm x 1mm   +44 (0) 1202...

    21 In Stock. £25.00 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details
  • 38.0 x 24.0 x 1.0mm

    38.0 x 24.0 x 1.0mm

    Product Code FSUVP38-24-1 UV Grade polished Fused Silica (SiO2) rectangular optical window 38mm x 24mm x 1mm   +44 (0) 1202 307650...

    8 In Stock. £30.00 each – for quantities of 10 or more, please phone to discuss discount.