Silica Glass UV - Circular Windows

Silica Glass UV - Circular Windows

UV Grade Fused Silica - Circular Windows.

Fused Silica normally contains OH which causes a strong absorption centred on 2.7μm limiting transmission to 2.2μm and restricting usefulness for IR applications. Grades with low OH (typically less than 10ppm) are available and they can be used effectively to 3.0μm.

These windows are made from UV grade material which contains OH and are useful from 0.18μmto 2.2μm.

Click for Technical Data on Silica Glass

  •  12.7mm x 1.6mm

    12.7mm x 1.6mm

    Product Code FSUVP12.7-1.6 UV Grade polished Fused Silica (SiO2) optical window 12.7mm Ø x 1.6mm (0.5" Ø x 1.6mm)   +44...

    35 In Stock. £12.00 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details
  •  13.0mm x 2.0mm

    13.0mm x 2.0mm

    Product Code FSUVP13-2 UV Grade polished Fused Silica (SiO2) optical window 13mm Ø x 2mm   +44 (0) 1202 307650 or...

    9 In Stock. £13.00 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details
  •  15.0mm x 1.0mm

    15.0mm x 1.0mm

    Product Code FSUVP15-1 UV Grade polished Fused Silica (SiO2) optical window 15mm Ø x 1mm   +44 (0) 1202 307650 or...

    14 In Stock. £19.00 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details
  •  20.0mm x 1.5mm

    20.0mm x 1.5mm

    Product Code FSUVP20-1.5 UV Grade polished Fused Silica (SiO2) optical window 20mm Ø x 1.5mm   +44 (0) 1202 307650 or...

    8 In Stock. £20.00 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details
  •  20.0mm x 2.0mm

    20.0mm x 2.0mm

    Product Code FSUVP20-2 UV Grade polished Fused Silica (SiO2) optical window 20.0(+0/-0.25)mm Ø x 2mm   +44 (0) 1202 307650...

    18 In Stock. £20.00 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details
  •  25.0mm x 1.0mm

    25.0mm x 1.0mm

    Product Code FSUVP25-1 UV Grade polished Fused Silica (SiO2) optical window 25.0mm Ø x 1mm   +44 (0) 1202 307650 or...

    66 In Stock. £19.00 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details
  •  25.0mm x 2.0mm

    25.0mm x 2.0mm

    Product Code FSUVP25-2 UV Grade polished Fused Silica (SiO2) optical window 25.0mm Ø x 2mm   +44 (0) 1202 307650 or...

    78 In Stock. £23.00 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details
  •  25.4mm x 1.0mm

    25.4mm x 1.0mm

    Product Code FSUVP25.4-1 UV Grade polished Fused Silica (SiO2) optical window 25.4mm Ø x 1mm (1" Ø x 1mm )   +44 (0) 1202...

    183 In Stock. £22.00 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details
  •  30.0mm x 2.0mm

    30.0mm x 2.0mm

    Product Code FSUVP30-2 UV Grade polished Fused Silica (SiO2) optical window 30mm Ø x 2mm   +44 (0) 1202 307650 or...

    8 In Stock. £27.00 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details
  •  32.0mm x 1.5mm

    32.0mm x 1.5mm

    Product Code FSUVP32-1.5 UV Grade polished Fused Silica (SiO2) optical window 32mm Ø x 1.5mm   +44 (0) 1202 307650 or...

    0 In Stock. £25.00 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details
  •  40.0mm x 2.0mm

    40.0mm x 2.0mm

    Product Code FSUVP40-2 UV Grade polished Fused Silica (SiO2) optical window 40mm Ø x 2mm   +44 (0) 1202 307650 or...

    0 In Stock. £30.00 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details