10.0mm Ø x 2.0mm
Polished Crystal Quartz (SiO2) optical window 10mm Ø x 2mm Z-cut Right Hand Rotation POA +44 (0) 1202 307650 or...
Quartz Crystal Windows from Stock.
These windows are all z-cut or zero degree with the optical axis perpendicular to the window surface.
Quartz exhibits a "handedness", normally this is Right-Handed but can be available also as Left-Handed on special request.
In normal use the handedness can be ignored.
Polished Crystal Quartz (SiO2) optical window 10mm Ø x 2mm Z-cut Right Hand Rotation POA +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) optical window 12mm Ø x 2mm Z-cut Right Hand Rotation POA +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) optical window 13mm Ø x 2mm Z-cut Right Hand Rotation POA +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) optical window 15mm Ø x 2mm Z-cut Right Hand Rotation POA +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) optical window 20mm Ø x 0.5mm Z-cut Right Hand Rotation +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) optical window 20mm Ø x 1mm Z-cut Right Hand Rotation +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) optical window 20mm Ø x 2mm Z-cut Right Hand Rotation +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) Optical window 25mm Ø x 1mm Z cut Right hand rotation +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) optical window 25mm Ø x 2mm Z-cut Right Hand Rotation +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) optical window 25mm Ø (+0/-0.1) x 2.5 (+/-0.1)mm Z-cut Right Hand Rotation Can be used in...
Polished Crystal Quartz (SiO2) optical window 25mm Ø (+0/-0.1) x 2.66 (+/-0.1)mm Z-cut Right Hand Rotation Can be used in...
Polished Crystal Quartz (SiO2) optical window 26mm Ø x 1mm Z-cut Right Hand Rotation +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) optical window 32mm Ø x 3mm Z-cut Right Hand Rotation +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) optical window 35mm Ø x 1mm Z-cut Right Hand Rotation +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) optical window 35mm Ø x 1.5mm Z-cut Right Hand Rotation +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) optical window 35mm Ø x 2mm Z-cut Right Hand Rotation +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) optical window 38mm Ø x 3mm Z-cut Right Hand Rotation +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) optical window 40mm Ø x 2mm Z-cut Right Hand Rotation +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) optical window 42mm Ø x 2mm Z-cut Right Hand Rotation +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) optical window 50mm Ø x 3mm Z-cut Right Hand Rotation +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) optical window 50.8mm Ø x 5mm (2 inch Ø x 5mm) Z-cut Right Hand Rotation +44 (0) 1202...
Polished Crystal Quartz (SiO2) optical window 60mm Ø x 2mm Z-cut Right Hand Rotation +44 (0) 1202 307650 or...
Polished Crystal Quartz (SiO2) optical window 80mm Ø x 3mm Z-cut Right Hand Rotation +44 (0) 1202 307650 or...