0 Items : £0.00

12.5mm Ø x 0.5mm VUV

12.5mm Ø x 0.5mm VUV

Product Code: LIFP12.5-0.5U

Price:
£65.00
19 In Stock
There is not enough stock to fulfil your order, either reduce the amount to the number available, or if you do require more, proceed and you will be contacted by a member of the sales team.
VUV grade Polished Lithium Fluoride (LiF) optical window
12.5mm Ø x 0.5mm
Guaranteed to give transmission T >40% at 121nm though 1mm
Typically T ~55% (T >60% supplied on request at a premium price)