15 x 15 x 15mm 45° Prism
IR Polished Calcium Fluoride (CaF2) 45° prism 15 x 15 x 15mm 45° right angle prism. +44 (0) 1202 307650 or [email protected] ...
Prisms from Stock
60° equilateral dispersing prisms
45° right angle reflective prisms
Normal production prisms are qualified for IR useage but can give good performance over most of the UV spectrum. For guaranteed transmission across the UV (and VUV) choose Stock Codes which end in U. Click here for our Guide to Calcium Fluoride Grades
IR Polished Calcium Fluoride (CaF2) 45° prism 15 x 15 x 15mm 45° right angle prism. +44 (0) 1202 307650 or [email protected] ...
IR Polished Calcium Fluoride (CaF2) 60° prism 15 x 15 x 15mm 60° equiliateral dispersing prism. +44 (0) 1202 307650 or...
IR Polished Calcium Fluoride (CaF2) 45° prism 25 x 25 x 25mm 45° right angle prism. +44 (0) 1202 307650 or [email protected] ...
*UV Grade* Polished Calcium Fluoride (CaF2) 45° prism 25 x 25 x 25mm 45° right angle prism. +44 (0) 1202 307650 or...
IR Polished Calcium Fluoride (CaF2) 60° prism 25 x 25 x 25mm 60° equiliateral dispersing prism. +44 (0) 1202 307650 or...
IR Polished Calcium Fluoride (CaF2) 45° prism 30 x 30 x 30mm 45° right angle prism. +44 (0) 1202 307650 or [email protected] ...
IR Polished Calcium Fluoride (CaF2) 60° prism 30 x 30 x 30mm 60° equiliateral dispersing prism. +44 (0) 1202 307650 or...