Calcium Fluoride Cylindrical Lenses

Calcium Fluoride Cylindrical Lenses

Calcium Fluoride Cylindrical Lenses from Stock

Click for Technical Data on Calcium Fluoride

  • 25 x 25 x 25 mm F.L. PCX

    25 x 25 x 25 mm F.L. PCX

    IR Polished Plano-convex (PCX) Calcium Fluoride (CaF2) hemi-cylindrical Lens 25mm x 25mm F.L. = 25mm @ 3μm nominal   ...

    5 In Stock. £160.00 each – for quantities of 10 or more, please phone to discuss discount.
    Buy NowView Details