Product Data

Transmission Range : 0.5 to 40 μm
Refractive Index : 2.338 at 10 μm (1)
Reflection Loss : 27.7% @ 10 μm
Absorption Coefficient : n/a
Reststrahlen Peak : 172 μm
dn/dT : n/a
dn/dμ = 0 : 8.5 μm
Density : 7.453 g/cc
Melting Point : 460 °C
Thermal Conductivity : 0.586 W m-1 K-1 at 343K
Thermal Expansion : 51 x 10-6 /°C at 300K
Hardness : Knoop 11.9 with 500g indenter
Specific Heat Capacity : 188 J Kg-1 K-1 (3)
Dielectric Constant : 30.3 at 1 MHz
Youngs Modulus (E) : 29.5 GPa (2)
Shear Modulus (G) : 7.58 GPa (2)
Bulk Modulus (K) : 22.47 GPa (2)
Elastic Coefficients : C11=37.8; C12=14.8; C44=7.56 (2)
Apparent Elastic Limit : 20.7 MPa (3000 psi)
Poisson Ratio : 0.281
Solubility : 0.05g/100g water ar 25°C
Molecular Weight : 248.31
Class/Structure : Cubic CsCl, Pm3m, no cleavage

To download this data or our MSDS safety data sheet as a pdf, please click on the links at the top of the page.  To expand the transmission graphs, please click on the image.

Images

Thallium Bromide IR Transmission Thallium Bromide Visible Transmission

Refractive Index

µm    No µm    No µm    No
0.438    2.652 0.546    2.452 0.578    2.424
0.650    2.384 0.750    2.350 10.00    2.338

Product Notes

Thallium Bromide crystals are grown by sealed-ampoule Stockbarger technique. Thallium salts are toxic, and Thallium Bromide has enough solubility to require extreme caution. Careful handling with plastic gloves covered with soft cotton gloves as appropriate to delicate optics is required.

REFERENCES:
(1) Handbook of Optical Constants, ed Palik, V3, ISBN 0-12-544423-0
(2) Arenberg, Measurements made at Naval Research Labs, USA 1948-49
(3) Kelly, Bureau of Mines Bulletin, No 371, p51. 1934
Data provided is extracted from our technical handbook of materials. While every attempt has been made to verify the source of the information, Crystran Ltd accept no responsibility for accuracy of data
Back to Materials
Popular Downloads
Calcium Fluoride
Barium Fluoride
Germanium
Lithium Fluoride
Magnesium Fluoride
Quartz
Sapphire
Silicon
Zinc Selenide
Zinc Sulphide Cleartran

Membership


Crystran Ltd is proud to be ISO 9001 certified through LRQA and ISO 14001 certified through SGS.
UKAS