Silver Bromide is useful material for very deep IR applications where sensitivity to moisture is a problem. Silver Bromide crystal growth was developed relatively recently by the standards of many IR materials. The parameters of Silver Bromide have not been researched as thoroughly as those of Silver Chloride. This soft crystal deforms under heat and pressure and can be forged in polished dies to create IR windows and lenses.

Product Data

Transmission Range : 0.45 to 35 μm (1)
Refractive Index : 2.167 at 10 μm (1)(2)
Reflection Loss : 23.9% at 10 μm (2 surfaces)
Absorption Coefficient : Not known
Reststrahlen Peak : 112.7 μm
dn/dT : Not known
dn/dμ = 0 : Not known
Density : 6.473 g/cc
Melting Point : 432 °C
Thermal Conductivity : 1.21 W m-1 K-1 at 273 K
Thermal Expansion : 30 x 10-6/°C at 273 K
Hardness : Knoop 7
Specific Heat Capacity : 292 J Kg-1 K-1
Dielectric Constant : 13.1 at 1MHz (2)
Youngs Modulus (E) : 31.97 GPa
Shear Modulus (G) ; Not Known
Bulk Modulus (K) : 44.03 GPa
Elastic Coefficients : C11=56.3 C12=32.3 C44=7.25
Apparent Elastic Limit : 26.2 MPa
Poisson Ratio : Not Known
Solubility : 12 x 10-6g/100g water at 20°C
Molecular Weight : 187.78
Class/Structure : Cubic FCC, NaCl, Fm3m, No cleavage, cold flows

To download this data or our MSDS safety data sheet as a pdf, please click on the links at the top of the page.  To expand the transmission graphs, please click on the image.

Images

Silver Bromide IR Transmission

Refractive Index

µm    No µm    No µm    No
0.391    2.416 0.477    2.33 0.496    2.313
0.55    2.27 0.6    2.25 0.65    2.24
0.781    2.205 9.926    2.167 12.66    2.162

Product Notes

Silver Bromide is grown in small ingots by sealed ampoule Stockbarger techniques. Silver Bromide is malleable and deep yellow, it darkens in sunlight, but less readiliy than Silver Chloride.

(1) Handbook of Optical Constants, ed Palik, V3, ISBN 0-12-544423-0
(2) White; Optical Properties of Silver Bromide. J.Opt.Soc. Am. V62, N2 (1973)
Data provided is extracted from our technical handbook of materials. While every attempt has been made to verify the source of the information, Crystran Ltd accept no responsibility for accuracy of data
Back to Materials
Popular Downloads
Calcium Fluoride
Barium Fluoride
Germanium
Lithium Fluoride
Magnesium Fluoride
Quartz
Sapphire
Silicon
Zinc Selenide
Zinc Sulphide Cleartran

Membership


Crystran Ltd is proud to be ISO 9001 certified through LRQA and ISO 14001 certified through SGS.
UKAS