Product Data

Transmission Range : 0.2 to 25 μm
Refractive Index : 1.46 at 10.6 μm
Reflection Loss : 6.8% at 10.6 μm (2 surfaces)
Absorption Coefficient : 1 x 10-3 cm-1 at 10.6  μm
Reststrahlen Peak : n/a
dn/dT : -39 x 10-6/°C
dn/dμ = 0 : n/a
Density : 2.8 g/cc
Melting Point : 715°C
Thermal Conductivity : 7.6 W m-1 K-1
Thermal Expansion : 36 x 10-6 /°C at 300K
Hardness : n/a
Specific Heat Capacity : 418 J Kg-1 K-1 at 283K
Dielectric Constant : 55
Youngs Modulus (E) : n/a
Shear Modulus (G) : n/a
Bulk Modulus (K) : 16.3 GPa
Elastic Coefficients : C11=36.4; C12=6.3; C44=4.7
Apparent Elastic Limit : n/a
Poisson Ratio : n/a
Solubility : 77g/100g water
Molecular Weight : 120.92
Class/Structure : Cubic FCC, NaCl, Fm3m, (100) cleavage

To download this data or our MSDS safety data sheet as a pdf, please click on the links at the top of the page.  To expand the transmission graphs, please click on the image.

Images

Rubidium Chloride IR Transmission Rubidium Chloride UV Transmission

Refractive Index

µm    No µm    No µm    No
0.248    1.60 0.351    1.53 0.488    1.50
0.590    1.49 0.633    1.49 1.060    1.48
1.550    1.48 2.800    1.48 10.60    1.46

Product Notes

Rubidium Chloride is produced by the sealed-ampoule Stockbarger technique.
Data provided is extracted from our technical handbook of materials. While every attempt has been made to verify the source of the information, Crystran Ltd accept no responsibility for accuracy of data
Back to Materials
Popular Downloads
Calcium Fluoride
Barium Fluoride
Germanium
Lithium Fluoride
Magnesium Fluoride
Quartz
Sapphire
Silicon
Zinc Selenide
Zinc Sulphide Cleartran

Membership


Crystran Ltd is proud to be ISO 9001 certified through LRQA and ISO 14001 certified through SGS.
UKAS