Magnesium Oxide (MgO) Data Sheet
Magnesium Oxide (MgO) MSDS

Magnesium Oxide (MgO)

Magnesium Oxide can be used for high temperature windows and substrates. HTSC substrates.

Product Data

Transmission Range : 0.3 to 6 μm
Refractive Index : 1.7085 at 2 μm (1)
Reflection Loss : 12.8% at 2 μm (2 surfaces)
Absorption Coefficient : 0.05 cm-1 at 5.5 μm
Reststrahlen Peak : n/a
dn/dT : +19 x 10-6 /°C
dn/dμ = 0 : n/a
Density : 3.58 g/cc
Melting Point : 2800 °C
Thermal Conductivity : 42 W m-1 K-1 at 273K
Thermal Expansion : 10.8 x 10-6 /°C at 273K
Hardness : Knoop 692 with 600g indenter
Specific Heat Capacity : 877 J Kg-1 K-1
Dielectric Constant : 9.65 at 1 MHz
Youngs Modulus (E) : 249 GPa
Shear Modulus (G) : 155 GPa
Bulk Modulus (K) : 155 GPa
Elastic Coefficients : C11=294; C12=93; C44=155
Apparent Elastic Limit : 138 MPA (20,000 psi)
Poisson Ratio : 0.18
Solubility : 0.00062g/100g Water
Molecular Weight : 40.32
Class/Structure : Cubic FCC, NaCl, Fm3m, (100) cleavage

To download this data or our MSDS safety data sheet as a pdf, please click on the links at the top of the page.  To expand the transmission graphs, please click on the image.

Images

Magnesium Oxide IR Transmission Magnesium Oxide UV Transmission

Refractive Index

µm    No µm    No µm    No
0.171    2.319 0.180    2.138 0.191    2.039
0.200    1.986 0.230    1.892 0.276    1.824
0.310    1.795 0.382    1.7668 0.436    1.75471
0.50    1.754 0.644    1.734 1.00    1.7229
2.00    1.7085 3.00    1.6915 4.00    1.6679
5.00    1.6373 6.02    1.5957 7.04    1.543
8.07    1.475 9.09    1.389 10.64    1.209

Product Notes

Magnesium Oxide is grown in relatively small sizes, mainly in Japan and China.

REFERENCES:
(1) Handbook of Optical constants of Solids II ISBN 0-12-544422-2
Data provided is extracted from our technical handbook of materials. While every attempt has been made to verify the source of the information, Crystran Ltd accept no responsibility for accuracy of data
Back to Materials
Popular Downloads
Calcium Fluoride
Barium Fluoride
Germanium
Lithium Fluoride
Magnesium Fluoride
Quartz
Sapphire
Silicon
Zinc Selenide
Zinc Sulphide Cleartran

Membership


Crystran Ltd is proud to be ISO 9001 certified through LRQA and ISO 14001 certified through SGS.
UKAS