Lead Fluoride has little optical application. Lead Fluoride has been used as a scintillator material as it has excellent stopping power for gamma rays.

Product Data

Transmission Range : 250nm to 11 μm
Refractive Index : 1.7808 @ 5 μm
Reflection Loss : 12.8% @ 5 μm (2 surfaces)
Absorption Coefficient : 0.018 cm-1 @ 4 μm
Reststrahlen Peak : n/a
dn/dT : n/a
dn/dμ = 0 : 3.3 μm
Density : 7.77 g cm-3 (1)
Melting Point : 855°C
Thermal Conductivity : n/a
Thermal Expansion : 29 x 10-6 K-1 @ 283K
Hardness : Knoop 200
Specific Heat Capacity : 301 J Kg-1 K-1
Dielectric Constant : 13 @ 1MHz
Youngs Modulus (E) : n/a
Shear Modulus (G) : n/a
Bulk Modulus (K) : n/a
Elastic Coefficients : C11=91, C12=46, C44=23
Apparent Elastic Limit : n/a
Poisson Ratio : n/a
Solubility : 0.064 g/100g water at 20°C
Molecular Weight : 245.21
Class/Structure : Cubic, CaF2, Fm3m, (111) cleavage

To download this data or our MSDS safety data sheet as a pdf, please click on the links at the top of the page.  To expand the transmission graphs, please click on the image.

Images

Lead Fluoride IR Transmission Lead Fluoride UV Transmission

Refractive Index

µm    No µm    No µm    No
0.3    1.93665 0.4    1.81804 0.5    1.78220
0.6    1.76489 0.7    1.75502 0.8    1.74879
0.9    1.74455 1.0    1.74150 3.0    1.72363
5.0    1.70805 7.0    1.68544 9.0    1.65504

Product Notes

Lead fluoride has been grown by vacuum Stockbarger, but is not known to be in regular production. Crystran hold a very small stock of crystal ingot.

REFERENCES
(1) Crystran Data 
WEBLINKS:
Shanghai Institute - Growth and Scintillator Properties.
Data provided is extracted from our technical handbook of materials. While every attempt has been made to verify the source of the information, Crystran Ltd accept no responsibility for accuracy of data
Back to Materials
Popular Downloads
Calcium Fluoride
Barium Fluoride
Germanium
Lithium Fluoride
Magnesium Fluoride
Quartz
Sapphire
Silicon
Zinc Selenide
Zinc Sulphide Cleartran

Membership


Crystran Ltd is proud to be ISO 9001 certified through LRQA and ISO 14001 certified through SGS.
UKAS