Lanthanum Fluoride (LaF3)

Lanthanum Fluoride is not often used as an optical material. Lanthanum Fluoride is usually doped with Europium at a nominal level of 0.3% mole. In this form, the usual application is as the active element in an ion-selective electrode for the detection and measurement of Fluoride ions in solution.

Product Data

Transmission Range : 0.2 to 11 μm
Refractive Index : No 1.506 at 0.55 μm
Reflection Loss : 10.3% at 0.55 μm
Absorption Coefficient : n/a
Reststrahlen Peak : n/a
dn/dT : n/a
dn/dμ = 0 : n/a
Density : 5.94
Melting Point : 1493 °C
Thermal Conductivity ; 5.1 W m-1 K-1 at 300K
Thermal Expansion ; 11 x 10-6 /K (para) 17 x 10-6 (perp)
Hardness ; Moh 4.5
Specific Heat Capacity : 506 J Kg-1 K-1
Dielectric Constant : n/a
Youngs Modulus (E) : n/a
Shear Modulus (G) : n/a
Bulk Modulus (K) : n/a
Elastic Coefficients : n/a
Apparent Elastic Limit : n/a
Poisson Ratio : n/a
Solubility : Insoluble in water
Molecular Weight : 195.9
Class/Structure : Trigonal (hex), P3cl, no cleavage

To download this data or our MSDS safety data sheet as a pdf, please click on the links at the top of the page.  To expand the transmission graphs, please click on the image.

Images

Lanthanum Fluoride IR Transmission Lanthanum Fluoride UV Transmission

Refractive Index

µm    No Ne µm    No Ne µm    No Ne
0.254    1.656 1.649 0.405    1.618 1.612 0.436    1.617 1.609
0.547    1.606 1.602

Product Notes

Lanthanum Fluoride is grown as small ingots of about 10mm diameter as it is difficult to anneal. Doped with Europium, it is a pale yellow colour.
Data provided is extracted from our technical handbook of materials. While every attempt has been made to verify the source of the information, Crystran Ltd accept no responsibility for accuracy of data
Back to Materials
Popular Downloads
Calcium Fluoride
Barium Fluoride
Germanium
Lithium Fluoride
Magnesium Fluoride
Quartz
Sapphire
Silicon
Zinc Selenide
Zinc Sulphide Cleartran

Membership


Crystran Ltd is proud to be ISO 9001 certified through LRQA and ISO 14001 certified through SGS.
UKAS