Product Data

Transmission Range : 0.4 to 30 μm
Refractive Index : 2.1723 at 11 μm (1)(3)
Reflection Loss : 24.0% at 11 μm (2 surfaces)
Absorption Coefficient : n/a
Reststrahlen Peak : 91.5 μm
dn/dT : n/a
dn/dμ = 0 : 5 μm
Density : 7.18 g/cc (3)
Melting Point : 423 °C (3)
Thermal Conductivity : 0.7 W m-1 K-1 at 329K
Thermal Expansion : 50 x 10-6 /°C (2)
Hardness : Knoop 29.9 with 500g indenter (2)
Specific Heat Capacity : 188 J Kg-1 K-1
Dielectric Constant : 32 at 1 MHz
Youngs Modulus (E) : 20.68 GPa (2)
Shear Modulus (G) : 8.48 GPa (2)
Bulk Modulus (K) : 22.81 GPa (2)
Elastic Coefficients : C11=38.5; C12=14.9; C44=7.37
Apparent Elastic Limit : 20.7 MPa (3000 psi)
Poisson Ratio : 0.219
Solubility : 0.3g/100g water at 20°C
Molecular Weight : 40 mole% TlBr; 60 mole% TlCl
Class/Structure : Cubic, CsCl structure, Pm3m, no cleavage (3)

To download this data or our MSDS safety data sheet as a pdf, please click on the links at the top of the page.  To expand the transmission graphs, please click on the image.

Images

KRS6 IR Transmission KRS6 VIS Transmission

Refractive Index

µm    No µm    No µm    No
0.6    2.3294 0.7    2.2982 0.8    2.2660
0.9    2.251 1.0    2.2404 1.5    2.2148
2.0    2.2059 3.0    2.199 4.0    2.1956
5.0    2.1928 6.0    2.190 7.0    2.187
8.0    2.1839 9.0    2.1805 10.0    2.1767
11.0    2.1723 12.0    2.1674 13.0    2.162
14.0    2.1563 15.0    2.1504 16.0    2.1442
17.0    2.1377 18.0    2.1309 19.0    2.1236
20.0    2.1154 21.0    2.1067 22.0    2.0976
23.0    2.0869 24.0    2.0752

Product Notes

KRS-6 crystals are grown by the sealed-ampoule Stockbarger technique. Starting materials of the highest purity are selected to ensure that there are no anionic absorption bands between 2 and 16 microns and all crystals are checked for quality by using a pathlength of 120mm. Thallium salts are toxic, and KRS6 has enough solubility to require extreme caution. Careful handling with plastic gloves covered with soft cotton gloves as appropriate to delicate optics is required.

REFERENCES:
(1) Hettner and Leisegang; Optik, V3, p305, 1948
(2) Combes, Ballard, McCarthy: J.Opt Soc.Am. V41, p 215, 1951
(3) Handbook of Optical Constants, ed Palik, V3, ISBN 0-12-544423-0
Data provided is extracted from our technical handbook of materials. While every attempt has been made to verify the source of the information, Crystran Ltd accept no responsibility for accuracy of data
Back to Materials
Popular Downloads
Calcium Fluoride
Barium Fluoride
Germanium
Lithium Fluoride
Magnesium Fluoride
Quartz
Sapphire
Silicon
Zinc Selenide
Zinc Sulphide Cleartran

Membership


Crystran Ltd is proud to be ISO 9001 certified through LRQA and ISO 14001 certified through SGS.
UKAS