KRS5 deep IR material with a high refractive index, KRS5 is used extensively in spectroscopy for ATR prisms, windows and lenses. In conjunction with Germanium, KRS5 can also be used in athermalised IR imaging systems.

Product Data

Transmission Range : 0.6 to 40 μm
Refractive Index : 2.371 at 10 μm (1)(3)
Reflection Loss : 28.4% at 10 μm (2 surfaces)
Absorption Coefficient : n/a
Reststrahlen Peak : n/a
dn/dT : -235 x 10-6 /°C
dn/dμ = 0 : 7 μm
Density ; 7.371 g/cc (3)
Melting Point : 414.5 °C (3)
Thermal Conductivity : 0.544 W m-1 K-1 at 293K
Thermal Expansion : 58 x 10-6 /°C (2)
Hardness : Knoop 40.2 (2)
Specific Heat Capacity : 200 J Kg-1 K-1 at 273K
Dielectric Constant : 32.5
Youngs Modulus (E) : 15.85 GPa (2)
Shear Modulus (G) : 5.79 GPa (2)
Bulk Modulus (K) : 19.78 GPa (2)
Elastic Coefficients : C11=331; C12=13.2; C44=5.79
Apparent Elastic Limit : 26.2 MPa (2)
Poisson Ratio : 0.369
Solubility : 0.05g/100g water at 293K
Molecular Weight : 42 mole% TlBr; 58 mole% TlI
Class/Structure : Cubic, CsCl structure, Pm3m, No cleavage (3)

To download this data or our MSDS safety data sheet as a pdf, please click on the links at the top of the page.  To expand the transmission graphs, please click on the image.

Click to access current KRS5 Stock Windows
Click to access current KRS5 Stock ATR Prisms 

Images

KRS5 IR Transmission KRS5 VIS Transmission

Refractive Index

µm    No µm    No µm    No
0.54    2.68059 1.00    2.44620 1.50    2.40774
2.00    2.39498 3.00    2.38574 4.00    2.38204
5.00    2.37979 6.00    2.37797 7.0    2.37627
8.0    2.37452 9.0    2.37267 10.0    2.37069
11.0    2.36854 12.0    2.36622 13.0    2.36371
14.0    2.36101 15.0    2.35812 16.0    2.35502
17.0    2.35173 18.0    2.34822 19.0    2.34451
20.0    2.34058 21.0    2.33643 22.0    2.33206
23.0    2.32746 24.0    2.32264 25.0    2.31758
26.0    2.31229 27.0    2.30676 28.0    2.30098
29.0    2.29495 30.0    2.28867 31.0    2.28212
32.0    2.27531 33.0    2.26823 34.0    2.26087
35.0    2.25322 36.0    2.24528 37.0    2.23705
38.0    2.22850 39.0    2.21965 40.0    2.21047

Product Notes

KRS-5 crystalises by the sealed-ampoule Stockbarger technique. Starting materials of the highest purity are selected to ensure that there are no anionic absorption bands between 2μm and 16μm and all crystals are checked for quality by using a pathlength of 120mm.
CAUTION: Thallium salts are considered TOXIC and should be handled with care.

REFERENCES
(1) Rodney and Malitson J.Opt Soc.Am. V46, p 956, 1953
(2) Combes, Ballard, McCarthy: J.Opt Soc.Am. V41, p 215, 1951
(3) Handbook of Optical Constants, ed Palik, V3, ISBN 0-12-544423-0
Data provided is extracted from our technical handbook of materials. While every attempt has been made to verify the source of the information, Crystran Ltd accept no responsibility for accuracy of data
Back to Materials
Popular Downloads
Calcium Fluoride
Barium Fluoride
Germanium
Lithium Fluoride
Magnesium Fluoride
Quartz
Sapphire
Silicon
Zinc Selenide
Zinc Sulphide Cleartran

Membership


Crystran Ltd is proud to be ISO 9001 certified through LRQA and ISO 14001 certified through SGS.
UKAS