Calcium Fluoride Windows from Stock. Please click on a particular stock line for details and pricing. There are two pages of listings, with the rectangular windows shown after the circular windows.
Normally windows are qualified for IR useage but can give good performance over most of the UV spectrum. For guaranteed transmission across the UV (and VUV) choose Stock Codes ending in U.
If in doubt, we can provide an actual transmission.
Stock codes which end in D are windows with drilled holes and intended for spectroscopic cells.
Additional to the regular stock lines listed below we publish a list of production overruns here:
|