Calcium Fluoride Windows

Calcium Fluoride Windows from Stock. Please click on a particular stock line for details and pricing. There are two pages of listings, with the rectangular windows shown after the circular windows.
Normally windows are qualified for IR useage but can give good performance over most of the UV spectrum. For guaranteed transmission across the UV (and VUV) choose Stock Codes ending in U.
If in doubt, we can provide an actual transmission.
Stock codes which end in D are windows with drilled holes and intended for spectroscopic cells. 
Additional to the regular stock lines listed below we publish a list of production overruns here:

Listing Products 1 to 50 of 92 in total.

Browse Pages: Previous 1 | 2 Next
Popular Downloads
Calcium Fluoride
Barium Fluoride
Germanium
Lithium Fluoride
Magnesium Fluoride
Quartz
Sapphire
Silicon
Zinc Selenide
Zinc Sulphide Cleartran

Membership


Crystran Ltd is proud to be ISO 9001 certified through LRQA and ISO 14001 certified through SGS.
UKAS