50 x 50 x 50mm 60° Prism : Stock Code PRISM50-60-SF10

50 x 50 x 50mm 60° equilateral dispersing prism.
SF10 Flint Glass
£90.00
Not in Stock
Please telephone or email to order
+44 (0) 1202 307650 or  sales@crystran.co.uk