Barium Fluoride Window BAFP41-23-4

41.0 x 23.0 x 4.0mm: Stock Code BAFP41-23-4

IR Polished Barium Fluoride (BaF2) optical window
41mm x 23mm x 4mm
Rectangular - A popular size for spectroscopy
Undrilled for use alone or as a pair with BAFP41-23-4D
NOTE: Tolerances on spectroscopic windows are ±2mm 
Note that these windows are sometimes plain rectangles and sometimes cut from 41mm Ø windows and so have rounded ends.
£110.00
In Stock
Please telephone or email to order
+44 (0) 1202 307650 or sales@crystran.co.uk

Images

BAFP41-23-4 Barium Fluoride Window
Data provided is extracted from our technical handbook of materials. While every attempt has been made to verify the source of the information, Crystran Ltd accept no responsibility for accuracy of data
Back to Barium Fluoride Windows
Popular Downloads
Calcium Fluoride
Barium Fluoride
Germanium
Lithium Fluoride
Magnesium Fluoride
Quartz
Sapphire
Silicon
Zinc Selenide
Zinc Sulphide Cleartran

Membership


Crystran Ltd is proud to be ISO 9001 certified through LRQA and ISO 14001 certified through SGS.
UKAS