25.4mm Ø x 250 mm F.L. PCX : Stock Code ZNSE25.4LENS250AR |
IR Polished Plano-convex (PCX) Zinc Selenide Lens
F.L. = 250mm @ 12μm nominal
AR/AR Coated - please enquire for specifications
£190.00
In Stock
Please telephone or email to order
|
|
|
|
|
|
Data provided is extracted from our technical handbook of materials. While every attempt has been made to verify the source of the information, Crystran Ltd accept no responsibility for accuracy of data |
|
Back to Zinc Selenide Positive Lenses
|
|
|