25.0mm Ø x 2.0mm : Stock Code ZNSP25-2 |
IR Polished Zinc Sulphide Multispectral (ZnS) optical window
IR Polished Zinc Sulfide Multispectral (ZnS) optical window
Multispectral (Water-white ZnS)
£56.00
In Stock
Please telephone or email to order
|
|
|
|
|
|
Data provided is extracted from our technical handbook of materials. While every attempt has been made to verify the source of the information, Crystran Ltd accept no responsibility for accuracy of data |
|